June 27, 2024
[ Method 1] Degreasing treatment. Commonly used solvents are: trichloroethylene, acetone, ethyl acetate and methyl ethyl ketone.
[
Method 2] After degreasing, in the following solution at 70
-75 °C Immersion for 5 min : sodium hydroxide 12 water 100 rinsed with cold water and then in the following solution 20 ° C   Dipping 5min: chromium oxide 10 100 over anhydrous sodium sulfate 2.8 Water rinse with cold water, then washed with distilled water, the 40 ° C   dry.
[
Method 3] After degreasing, in 6.3% sodium hydroxide solution
70 ° C   After immersing for 10 min , washing with water, and then in the following solution 55 ° C Immersion for 5 min : chromium oxide 13.8 calcium sulfate 1.2 water 85 washed with distilled water, and then in the following solution 55 ° C Immersion for 3 min : chromium oxide 10 sodium sulfate 0.5 water 89.5 after washing with water 60 ° C   Dry below.
[
Method 4] in the following solution
20 ° C   Immersion for 3 min : chromium oxide 16.6 sodium nitrate 20 glacial acetic acid 105 water 100 rinsed with cold water, washed with distilled water, at 40 ° C   Dry below
[
Method 5] in the following solution at 60
-70 °C Dipping 3min: Sodium dichromate, manganese sulfate 10 5 5 Magnesium sulfate 80 water rinse with cold water, distilled water, in 70 ° C   Dry below.
[
Method 6] After degreasing, it was immersed in the following boiling solution for 20 minutes : sodium dichromate 1.5 ammonium sulfate 3 ammonia water (d = 0.88) 0.3 water 93.7 was rinsed with warm water, washed with distilled water, and dried.
[
Method 7] In
30 ° C   The following ammonium hydride ammonium 10% solution is anodized to a current density lower than 0.45A /m2 (one electrode panel), AC voltage 90-120V , then washed with water and dried.
[
Method 8] at 20
-30 °C Following anodization solution: potassium aluminum 12 0.75 3.4 sodium phosphate, potassium fluoride, anhydrous potassium permanganate 3.4   1.5 water 80 AC voltage 85V , current density 1.1 -1.4A /m2 , then washed with cold distilled water and dried.
[
Method 9] After degreasing
70 ° C   Wash the following lye for 5-15min : sodium hydroxide 23-34 water 400 is washed with cold water for 5min , then immersed in the following solution for 5-15min , temperature 55 ° C   : chrome oxide 57-68 calcium nitrate 5 water 450 washed with cold water for 2min , and then immersed in the following solution for 3-12min , temperature 55 ° C   : chrome oxide 45 sodium phosphate 8 water 450 washed in cold water for 2min , then 40 ° C   Dry for 30 min .  
எங்களை தொடர்பு கொள்ள

Author:

Mr. shamorawheels

Phone/WhatsApp:

13152747272

பிரபலமான தயாரிப்புகள்
You may also like
Related Categories

இந்த சப்ளையருக்கு மின்னஞ்சல் செய்யவும்

பொருள்:
மின்னஞ்சல்:
செய்தி:

Your message must be betwwen 20-8000 characters

பதிப்புரிமை © 2025 Shamora Material Industry அனைத்து உரிமைகளும் பாதுகாக்கப்பட்டவை.
நாங்கள் உங்களை உடனடியாக தொடர்புகொள்வோம்

உங்களுடன் வேகமாக தொடர்பு கொள்ளக்கூடிய கூடுதல் தகவல்களை நிரப்பவும்

தனியுரிமை அறிக்கை: உங்கள் தனியுரிமை எங்களுக்கு மிகவும் முக்கியமானது. உங்கள் வெளிப்படையான அனுமதிகளுடன் எந்தவொரு விரிவாக்கத்திற்கும் உங்கள் தனிப்பட்ட தகவல்களை வெளியிட வேண்டாம் என்று எங்கள் நிறுவனம் உறுதியளிக்கிறது.

அனுப்பு